地坪漆厂家关于环氧地坪漆常见固化问题总结

返回列表 来源: 浏览:176 发布日期:2019-6-1 20:32:44

环氧地坪漆常见的固化问题主要有:固化不均、固化不良、表面发黏、表面发白和不固化。下面环氧地坪漆厂家就给大家分析环氧地坪漆常见固化问题的原因。环氧地坪漆漆膜部分出现软和硬的涂膜状态。这主要是环氧地坪材料主漆与固化剂在混合容器里搅拌不良,混合不均匀。环氧地坪漆厂家建议大家在进行配料时采用搅拌器充分搅拌再使用。

The common curing problems of epoxy floor paint are uneven curing, poor curing, surface sticking, surface whitening and non-curing. The following epoxy floor paint manufacturers will give you an analysis of the reasons for the common curing problems of epoxy floor paint. 

1、固化不均

1. Non-uniform curing

环氧地坪漆漆膜部分出现软和硬的涂膜状态。这主要是地坪材料主漆与固化剂在混合容器里搅拌不良,混合不均匀。地坪漆厂家建议大家在进行配料时采用搅拌器充分搅拌再使用。

The film of epoxy floor paint is soft and hard. This is mainly due to the poor mixing and uneven mixing of the main paint and curing agent in the mixing container. Floor paint manufacturers recommend that we use mixer to mix and reuse the ingredients.

2、固化不良

2. Poor curing

整个漆膜固化状态差,重物或人员走动有压痕。这种现象主要是施工环境温度太低、反应不完全,或固化剂加入比例不符。光磊地坪漆厂家提醒大家地坪漆最佳施工温度是在5-35℃,配料时采用电子秤严格按照配比进行调配材料。

The whole film is in poor solidification state, and there are indentations in the movement of heavy objects or personnel. This phenomenon is mainly due to the construction environment temperature is too low, the reaction is not complete, or the proportion of curing agent does not match. Guanglei floor paint manufacturer reminds you that the best construction temperature of floor paint is 5-35 C. When mixing, electronic scales are used to mix materials strictly according to the proportion.

3、表面发黏不干

3. Surface stickiness

初凝时,环氧地坪漆表面发黏。主要原因是整个涂料的搅拌不充分,造成未反应的成分在表面下游离。

The surface of epoxy floor paint sticks when it is first set. The main reason is the inadequate stirring of the whole coating, which causes the unreacted components to be separated from the surface.

4、表面发白

4. Surface whitening

环氧地坪漆表面仿佛有层云雾。这主要是因为施工环境潮气重,涂膜上易结霜,或固化剂含水,使得固化剂里的胺析出产生白雾集结在表面。

There seems to be a cloud on the surface of epoxy floor paint. This is mainly due to the heavy humidity of the construction environment, the easy frosting on the coating, or the moisture content of the curing agent, which makes the amine precipitation in the curing agent produce white fog on the surface.

5、不固化

5. Non-curing

环氧地坪漆施工后一直不固化。主要原因是固化剂加量不准或加错;环境温度过低(低于5℃以下)。

Epoxy floor paint does not solidify after construction. The main reason is that the dosage of curing agent is inaccurate or wrong; the ambient temperature is too low (below 5 C).