环氧地坪漆有哪些优缺点与缺点对比?
在进行环氧地坪漆施工的过程中,会有起痱子的现象出现,很多人会问环氧地坪漆起痱子难道是因为天热么?环氧地坪漆起痱子是比较复杂,主要原因是溶剂保留以及水分的作用导致,环氧地坪漆在较高温度的情况下,剧烈的溶剂挥发和较强的溶剂保留造成溶剂蒸汽的滞留在涂膜内从而就导致痱子的产生;在比较低的温度下,涂膜的流动性比较差,溶剂的挥发造成温度偏低也会造成溶剂蒸汽滞留。
In the process of epoxy floor paint construction, there will be a rash phenomenon, many people will ask whether the rash is caused by hot weather? Epoxy flooring paint prickles are more complex, mainly due to solvent retention and the role of water. At higher temperatures, violent solvent volatilization and strong solvent retention cause solvent vapor to stay in the film, which leads to prickles. At lower temperatures, the flow of the film. Relatively low in temperature, solvent evaporation causes low temperature and also causes solvent vapor retention.
针对地坪漆起痱子的现象有以下预防措施:
According to the phenomenon of prickly heat on floor paint, the following precautionary measures are taken:
1、使用正确的稀释剂和固化剂
1. Use the right thinner and curing agent.
2、改善涂膜的干性来改变涂膜溶剂的稀释性。
2, improve the coating's dry property to change the dilution of the coating solvent.
3、使用正确的助剂,从而改善表面的透气性能。
3, use the right auxiliaries to improve the surface permeability.
4、最好减少低温下施工情况
4, best to reduce construction conditions at low temperatures.
5、降低溶剂极性,使涂膜对溶剂的保留能力降低。
5, reduce the polarity of solvents, so that the retention ability of film to solvent is reduced.
地坪漆起痱子我们需要对症下药,对于地坪漆施工过程中也希望我们认真对待每个细节也会减少很多不必要麻烦。
We need to prescribe the right remedy for the prickly rash of floor paint. We also hope that we will take every detail seriously in the process of floor paint construction and reduce a lot of unnecessary trouble.