现在很多人按照地板的时候,都会选择环氧自流平地面,这是属于大工程,需要很多方面的施工技术,怎样判断环氧自流平的质量以及环氧自流平地面做法有哪些,下面就来为大家详细介绍下吧!怎么判断环氧自流平地坪质量:1、环氧自流平地坪是一种无溶剂、自流平、粒子致密的厚浆型的地坪。它具有自动找平、耐磨、耐压的性能特点和高洁净、美观的环境要求,近几年来受到不少行业的 好评和应用。

Now many people will choose epoxy self-leveling floor according to the floor time, this is a large project, need a lot of construction technology, how to judge the quality of epoxy self-leveling and epoxy self-leveling floor practices, the following is to introduce in detail for you! How to judge the quality of epoxy self-leveling floor: 

1, the epoxy self leveling floor is a solvent-free, self leveling, dense particle thick flooring. It has the characteristics of automatic leveling, wear resistance, pressure resistance and high clean and beautiful environmental requirements. In recent years, it has been praised and applied by many industries.

2、环氧自流平的性能是无可挑剔的,但是由于施工技术和涂料本身的质量问题,导致自流平地坪的质量差异也非常显著。下面从三个方面为大家介绍在验 收时怎样判断环氧自流平的质量优劣。

2. The performance of epoxy self-leveling is impeccable, but the quality difference of self-leveling floor is very significant because of the quality problems of construction technology and coating itself. Here are three aspects to introduce how to judge the quality of epoxy self leveling during acceptance.

3、表面状况环氧自流平地坪是一种表面平滑、美观,具有优秀装饰效果的一种地坪,所以在验收的时候,要看清楚地坪表面是否平整、光亮可达镜面效果,且不能含 有颗粒等杂物。

3. Surface condition Epoxy self-leveling floor is a kind of surface smooth, beautiful, with excellent decorative effect of a kind of floor, so in acceptance, to see clearly whether the surface of the flat, bright mirror effect, and can not contain particles and other impurities.

4、丰满度丰满度即是看地面的反光率是否能达到95%,是否够饱满。这个指标在以前是不受到重视的,但是随着社会的进步和人们的要求逐渐提高,这一项指标也 渐渐变成了一项基本的技术要求。一般反射率达不到85%的都是不合格的。

4, fullness and fullness is to see whether the reflection rate of the ground can reach 95%, and whether it is full enough. This index was not taken seriously in the past, but with the progress of society and people's requirements gradually improved, this index has gradually become a basic technical requirements. Less than 85% of the total reflectance is unqualified.

5、硬度为了使地面有足够的耐磨性,许多客户都会要求地坪表面有一定的硬度。为了达到工业的使用要求,我们一般要求地坪的硬度大于2H。但是填料容易下沉的 自流平固化后的硬度并不是太高,所以要选填料不易下沉的为佳。

5. Hardness in order to make the ground have enough wear resistance, many customers will require the surface of the floor has a certain degree of hardness. In order to meet the requirements of industrial use, we generally require that the hardness of the floor is greater than 2H. But the hardness of the self-leveling solidified filler is not too high, so it is better to choose the filler which is not easy to sink.

环氧自流平

Epoxy self leveling

环氧自流平地面做法:

Epoxy self leveling ground practice:

(1)、施工人员将配料用容器和施工工具清洗干净,置于指定地点,在以后的施工过程中,随时配合,保证容器工具清洁、干燥、无油污、无固化残渣等。

(1) The constructors clean the ingredients with containers and construction tools and place them in the designated place. During the later construction, they should cooperate with each other at any time to ensure that the containers and tools are clean, dry, free of oil pollution and solidified residue.

(2)、计量工将称量好的树脂底涂料放入搅拌容器中,并做好记录用量,也应记录当时的温度、湿度,搅拌工预先搅拌好。

(2) Metrologists will weigh the good resin primer into the mixing container, and do a good job of recording dosage, should also record the temperature, humidity, mixer pre-mixing.

(3)、计量工按配合比准确称量好固化剂,并放入搅拌容器中,同时将用量做好记录,搅拌工继续搅拌,至少搅拌3分钟,以保证混合物均匀。

(3) Metrologists accurately weigh the curing agent according to the mixing ratio and put it into the mixing container. At the same time, the dosage is recorded. The mixer continues to mix for at least 3 minutes to ensure the uniformity of the mixture.

(4)、操作工将搅拌的混合物倒在施工区域内,用镘刀涂直至均匀,不得有空鼓、气泡等缺陷。

(4) Operators pour the mixture into the construction area and apply it with a trowel until it is uniform, and there must be no hollow or bubble defects.

(5)、在底涂未完成固化前不要开始涂表层,否则会起皱。

(5) do not begin to coat the surface before finishing the finish, otherwise it will wrinkle.

(6)、层间涂刷间隔时间视温度而定,若超过7天,涂面须以软毛刷或研磨机粗糙化,再涂表层以增加附着力。

(6) The interval between layers depends on the temperature, if more than 7 days, the surface should be roughened by soft brush or grinder, and then coated with surface layer to increase adhesion.

(7)、底漆保养时间为一般12小时后,确认硬化状态,进行下一道涂抹工序。

(7) when the primer is maintained for 12 hours, confirm the hardening state and carry out the next smearing process.